We fire clay (bisque) and glazed ceramics at low, medium, and high temperatures.
The kiln is 120 liters,top-loaded with a circular design. The maximum dimensions of the pieces being fired cannot exceed a diameter of 46 cm and a height of 60 cm (9 shelves).
o demonstrate the kiln's capacity, we have tested that it can hold 60 mugs with handles (10 cm in diameter, 10 cm in height) arranged on 5 shelves.

120-liter kiln – shelf diameter 42 cm, maximum width 46 cm, height 60 cm.

  • Bisque firing up to 1000 degrees Celsius
  • 1/2 kiln 80 PLN
  • whole kiln 120 PLN
  • szkliwo 1050 stopni
  • 1/2 kiln 90 PLN
  • whole kiln 140 PLN
  • szkliwo 1150 stopni
  • 1/2 kiln 100 PLN
  • whole kiln 160 PLN
  • szkliwo 1240 stopni
  • 1/2 kiln 105 PLN
  • whole kiln 170 PLN

 

Single items

  • 10x10x10
  • 12 PLN bisque
  • 15 PLN glaze 1050
  • 20 PLN glaze 1150
  • 22 PLN glaze 1240
  • 15x15x15
  • 22 PLN bisque
  • 25 PLN glaze 1050
  • 30 PLN glaze 1150
  • 32 PLN glaze 1240
  • Cleaning the shelf after glaze drips 80 PLN
  • Completely destroyed shelf 160 PLN

Additional information
- Pieces should be delivered during Klik Ceramika's opening hours
- Firing of pieces will occur at the earliest available time (to be confirmed by phone).
- Please avoid glazing the areas where the pieces will touch the kiln shelf.
- Pieces not cleaned of glaze from the bottom will not be fired.
- Pieces must be dry and ready for loading into the kiln upon arrival (glazing should be done at least one day in advance).
- Compensation for pieces damaged before firing will be equivalent to the accepted value for firing a piece of that size, to be used towards a future service.
- Hanging pieces are fired on a bead rack (please provide your own).
- Uncollected pieces within a month will be either destroyed or put up for sale.
- If the kiln shelf is soiled with glaze, a cleaning fee will be charged. If glaze application is improper and the shelf cannot be cleaned, the client will be charged for the entire shelf, according to the price list.
- In the case of kiln damage, the cost will be based on the specialist's assessment.

By leaving ceramic pieces for firing, the client accepts the above regulations.